Cast-iron – bronze plate – fractured at a weak area in the cast. The fractured area was tapped out and reinforced with a custom 3mm post to marry the two pieces. Then seizing compound was applied to fuse the two pieces together…
Finished with a little metallic touch up paint and off to a happy customer…